AJ04 – Stress Corrosion Cracking of Control Arm Shafts – 2015 Porsche 918 Spyder

Porsche Cars North America, Inc. (Porsche) is recalling certain 2015 Porsche 918

DTC Quick Navigation

If the control arm connecting shafts crack, affecting vehicle handling, it can increase the risk of a crash.

NHTSA Campaign Number: 18V287

Manufacturer Porsche Cars North America, Inc.

Components SUSPENSION

Potential Number of Units Affected 305

Summary

Porsche Cars North America, Inc. (Porsche) is recalling certain 2015 Porsche 918 Spyder vehicles. The connecting shafts of the longitudinal and transverse control arms may fail due to stress corrosion cracking, impacting vehicle handling.

Remedy

Porsche will notify owners, and dealers will replace the longitudinal and transverse control arms, free of charge. The manufacturer has not yet provided a notification schedule. Owners may contact Porsche customer service at 1-800-767-7243. Porsche’s number for this recall is AJ04.

Notes

Owners may also contact the National Highway Traffic Safety Administration Vehicle Safety Hotline at 1-888-327-4236 (TTY 1-800-424-9153), or go to www.safercar.gov.